Surface treatment
Phosphating
Inner treatment
Internal Epoxy Coating
Thermal Performance(℃ )
≤ 5
Bondingsurfaceporosity
1~4
The section void ratio
1~3
Resistance to deflection
No cracking
Salt fog resistance(1000h)
No change of anti-corrosion coating